INCOLOY Alloy 890 Alloy Round Bar Superalloy High Strength

Mianyang Baoheng New Material Technology Co.,Ltd
Contact Now

INCOLOY Alloy 890 Alloy Round Bar Superalloy High Strength

  • 1
  • 2

Brand Name : PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL

Model Number : INCOLOY alloy 890

Certification : SGS,TUV,BV,ISO,MTC

Place of Origin : China

MOQ : Negotiations

Price : Negotiations

Payment Terms : T/T

Supply Ability : 100000KGS/Month

Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 45-55days

Packaging Details : Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement

Product Name : INCOLOY alloy 890 Alloy Round Bar

Grades : INCOLOY alloy 890

Processing methods : Shot blasted,Peeled,Machined,etc

Surface : Black,Rrough Turned,etc

Profile : Round Bar,Forging Parts,etc

Price Term : Ex-work,FOB etc.

Contact Now

INCOLOY alloy 890 Alloy Round Bar 890 Superalloy Round Bar 890 Round Bar 890 Bar

Description

Our company provides INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.

All of INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

  • Material:Metal,INCOLOY alloy 890 Alloy Round Bar 890 Superalloy Round Bar 890 Round Bar 890 Bar
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Length: Fixed length or random length or based on the customer's special requirement.

Products Details

INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.10
Si (%): ≤ 1.80
Mn (%): ≤ 1.00
Cr (%):≤ 25.0
Ni (%):≤ 42.5
Mo (%): ≤15.0

Al (%): ≤0.70
Cu (%): ≤0.75

Ti(%): ≤1.00

Fe(%): Remainder

Form: bar and rod
Condition: cold worked and hot worked, annealed, at 1150 Deg. min.
Tensile strength,σb/≥ MPa: 520
Yield strength, σ0.2/≥ MPa: 205
Elongation, δ ≥(%): 35.0
Reduction of area, ф ≥ (%): -
Hardness | HRC: -
Service temperature: above 593 Deg

INCOLOY Alloy 890 Alloy Round Bar Superalloy High Strength

Applications:

INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.

Superalloy is widely used to produce the high temperature components for gas turbine in the field of aviation, naval vessels and industry:
Heat treating fixture
Furnace muffle
Nuclear reactor
Turbine engine parts - mechanical gears, gear shaft, main axis, blade
Mechanical parts - bolt and nut, fastener
Gas turbine,etc

INCOLOY Alloy 890 Alloy Round Bar Superalloy High StrengthINCOLOY Alloy 890 Alloy Round Bar Superalloy High Strength

INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.

FAQ

Q: How do you control the quality?

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar. and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

INCOLOY Alloy 890 Alloy Round Bar Superalloy High Strength


Product Tags:

high strength Alloy Round Bar

      

INCOLOY alloy 890 Alloy Round Bar

      

INCOLOY alloy 890

      
Quality INCOLOY Alloy 890 Alloy Round Bar Superalloy High Strength for sale

INCOLOY Alloy 890 Alloy Round Bar Superalloy High Strength Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Mianyang Baoheng New Material Technology Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)